Micromechanics of a functionally graded superalloy
The aim of this project is to characterise and understand components of Ni superalloys in coated systems using high fidelity micromechanical tests.
The techniques adopted include TEM, FIB, EBSD, in-situ micromechanical testing and synchrotron X-ray diffraction. These techniques will be employed to characterise and study the mechanics and key properties of the material in different crystallographic orientations.